Material – ASTM B 163 N08825
Standard Specification for Seamless Nickel and Nickel Alloy Condenser and Heat- Exchanger Tube
Group - Non-Ferrous Nickel Alloys
Sub Group - ASTM B 163 N08825 Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tube
Application - Intended for Valve, Pump, General Engineering, Automotive and other Industries
Grade Belongs to the Industry - Tube
| Chemical Composition | ||
|---|---|---|
| Carbon | C % | 0.050 max. |
| Silicon | Si % | 0.500 max. |
| Manganese | Mn % | 1.000 max. |
| Copper | Cu % | 1.500 - 3.000 |
| Sulphur | S % | 0.030 max. |
| Chromium | Cr % | 19.500 - 23.500 |
| Aluminium | Al % | 0.200 max. |
| Titanium | Ti % | 0.600 - 1.200 |
| Molybdenum | Mo % | 2.500 - 3.500 |
| Iron | Fe % | 22.000 max. |
| Nickel | Ni % | 38.000 - 46.000 |
| - | - | - |
| - | - | - |
| - | - | - |
| - | - | - |
| Heat Treatment |
|---|
| As-Cast or Annealing or Age Hardning |
| Mechanical Properties | |
|---|---|
| Tensile Strength in Mpa | 586 - 793 |
| Yield Strength in Mpa | 241 min. |
| Elongation in % | 5 min. |
| Reduction of Area in % | - |
| Hardness in HRC | 25 - 90 |
| Impact in Joule | - |
Cross Reference Table
| Material | Standard | Country | Grade Belong to the Industry |
|---|---|---|---|
| B 423 N08825 | ASTM | USA | Pipe and Tube |
| B 564 N08825 | ASTM | USA | Forging |
| B 704 N08825 | ASTM | USA | Tube |
| B 705 N08825 | ASTM | USA | Pipe |
| SB-163 N08825 | ASME | USA | Tube |
| - | - | - | - |
| - | - | - | - |