Material ‐ ASTM B148 C95800

Standard Specification for Aluminum - Bronze Sand Casting

Group - Non ‐ Ferrous Copper Alloy

Sub Group - ASTM B148 Aluminum ‐ Bronze Sand Casting

Application - Intended for Valve, Pump, General Engineering, Automotive and Other Industries

Grade Belongs to the Industry - Casting

Chemical Composition Heat Treatment
Aluminium Al % 8.500 ‐ 9.500
Iron Fe % 3.500 ‐ 4.500
Manganese Mn % 0.800 ‐ 1.500
Ni + Co Ni% + Co% 4.000 ‐ 5.000 As ‐ Cast
Lead Pb % 0.030 max.
Silicon Si % 0.100 max.
Copper Cu % 79.000 min.
Mechanical Properties
Tensile Strength in Mpa 585 min.
Yield Strength in Mpa 240 min.
Elongation in % 15 min.
Reduction of Area in %
Hardness in BHN
Impact in Joule

Cross Reference Table

Material Standard Country Grade Belong to the Industry
C95800 UNS USA Rod, Bar, Tube and Shapes
B271 C95800 ASTM USA Casting
SB ‐ 148 C95800 ASME USA Casting
SB ‐ 505 C95800 ASME USA Casting
C95800 SAE USA Casting
CACIn703 KS Korea Ingot and Casting
B505 C95800 ASTM USA Casting