Material – DIN 2.4180

Standard Specification for Nickel and Nickel-Copper Alloy Casting

Group - Non-Ferrous Nickel Alloys

Sub Group - DIN 2.4180 Nickel and Nickel-Copper Alloy Casting

Application - Intended for Valve, Pump, General Engineering, Automotive and other Industries

Grade Belongs to the Industry - Casting

Chemical Composition
CarbonC %1.000 max.
SiliconSi %5.500 - 6.500
ManganeseMn %1.500 max.
CopperCu %1.200 max.
IronFe %1.000 max.
OtherOt%0.200 max.
Ni + CoNi% + Co%90.000 min.
---
---
---
---
---
---
---
---
Heat Treatment
As-Cast or Annealing or Age Hardning
Mechanical Properties
Tensile Strength in Mpa500 min.
Yield Strength in Mpa350 min.
Elongation in %3 min.
Reduction of Area in %-
Hardness in HRB180 min.
Impact in Joule-

Cross Reference Table

Material Standard Country Grade Belong to the Industry
G-Ni90Si DIN Germany Casting
- - - -
- - - -
- - - -
- - - -
- - - -
- - - -