Material – DIN 2.4632

Standard Specification for Nickel and Nickel Alloy Casting

Group - Non-Ferrous Nickel Alloys

Sub Group - DIN 2.4632 Nickel and Nickel Alloy Casting

Application - Intended for Valve, Pump, General Engineering, Automotive and other Industries

Grade Belongs to the Industry - Casting

Chemical Composition
CarbonC %0.130 max.
SiliconSi %1.000 max.
ManganeseMn %1.000 max.
ChromiumCr %18.000 - 21.000
AluminiumAl %1.000 - 2.000
BoronB %0.020 max.
CopperCu %0.200 max.
CobaltCo %15.000 - 21.000
IronFe %1.500 max.
PhosphorusP %0.020 max.
SulphurS %0.015 max.
TitaniumTi %2.000 - 3.000
ZirconiumZr %0.150 max.
NickelNi %Balance
---
Heat Treatment
As-Cast or Annealing or Age Hardning
Mechanical Properties
Tensile Strength in Mpa1100 min.
Yield Strength in Mpa700 min.
Elongation in %15 min.
Reduction of Area in %-
Hardness in BHN-
Impact in Joule-

Cross Reference Table

Material Standard Country Grade Belong to the Industry
- - - -
- - - -
- - - -
- - - -
- - - -
- - - -
- - - -