Material – DIN EN 1982 CuSn12-C
Standard Specification for Copper and Copper Alloys - Ingots and Castings
Group - Non-Ferrous Copper Alloy
Sub Group - DIN EN 1982 Copper and Copper Alloys - Ingots and Castings
Application - Intended for Valve, Pump, General Engineering, Automotive and Other Industries
Grade Belongs to the Industry - Ingot and Casting
| Chemical Composition | ||
|---|---|---|
| Aluminium | Al % | 0.010 max. |
| Iron | Fe % | 0.200 max. |
| Manganese | Mn % | 0.200 max. |
| Nickel | Ni % | 2.000 max. |
| Phosphorus | P % | 0.600 max. |
| Lead | Pb % | 0.700 max. |
| Sulphur | S % | 0.050 max. |
| Antimony | Sb % | 0.150 max. |
| Silicon | Si % | 0.010 max. |
| Tin | Sn % | 11.000 - 13.000 |
| Zinc | Zn % | 0.500 max. |
| Cu + Ni | Cu%+Ni% 85.000 - 88.500 | Elongation in % |
| - | - | - |
| - | - | - |
| - | - | - |
| Heat Treatment |
|---|
| As-Cast |
| Mechanical Properties | |
|---|---|
| Tensile Strength in Mpa | 260 - 300 |
| Yield Strength in Mpa | 140 - 150 |
| 5 - 7 | - |
| Reduction of Area in % | - |
| Hardness in HB | 80 - 90 |
| Impact in Joule | - |
Cross Reference Table
| Material | Standard | Country | Grade Belong to the Industry |
|---|---|---|---|
| CB483K | BS | British | Ingot and Casting |
| CC483K | AFNOR NF | France | Ingot and Casting |
| CC483K | ONORM | Australia | Ingot and Casting |
| CC483K | BDS | Bulgaria | Ingot and Casting |
| CC483K | UNI | Italy | Ingot and Casting |
| CuSn12-C | UNE | Spain | Ingot and Casting |
| CuSn12-C | MSZ | Hungary | Ingot and Casting |