Material – DIN EN 12164 CuZn37Pb1Sn1 (CW714R)

Standard Specification for Copper and Copper Alloy Rod for Free Machining Purpose

Group - Non Ferrous Copper Alloys

Sub Group - DIN EN 12164 CuZn37Pb1Sn1 Copper and Copper Alloy Rod for Free Machining Purpose

Application - Intended for Valve, Pump, General Engineering, Automotive and Other Industries

Grade Belongs to the Industry - Rod

Chemical Composition
IronFe %0.100 max.
NickelNi %0.300 max.
LeadPb %0.400 - 1.000
TinSn %0.500 - 1.000
OtherOt %0.200 max.
CopperCu %59.000 - 61.000
ZincZn %Balance
---
---
---
---
---
---
---
---
Heat Treatment
As Raw or Solution Heat Treated
Mechanical Properties
Tensile Strength in Mpa410 min.
Yield Strength in Mpa250 min.
Elongation in %12 min.
Reduction of Area in %-
Hardness in HV125 min.
Impact in Joule-

Cross Reference Table

Material Standard Country Grade Belong to the Industry
C 4622 BF JIS Japan Rod and Bar
CuZn37Pb1Sn1 ONORM Australia Rod
CW714R ONORM Australia Rod
CuZn37Pb1Sn1 NBN Belgium Rod
CW714R NBN Belgium Rod
CuZn37Pb1Sn1 EN European Union Rod
CW714R EN European Union Rod