Material – DIN EN 12164 CuZn37Mn3Al2PbSi (CW713R)

Standard Specification for Copper and Copper Alloy Rod for Free Machining Purpose

Group - Non Ferrous Copper Alloys

Sub Group - DIN EN 12164 CuZn37Mn3Al2PbSi Copper and Copper Alloy Rod for Free Machining Purpose

Application - Intended for Valve, Pump, General Engineering, Automotive and Other Industries

Grade Belongs to the Industry - Rod

Chemical Composition
AluminiumAl %1.300 - 2.300
IronFe %1.000 max.
ManganeseMn %1.500 - 3.000
NickelNi %1.000 max.
LeadPb %0.200 - 0.800
SiliconSi %0.300 - 1.300
TinSn %0.400 max.
OtherOt %0.300 max.
CopperCu %57.000 - 59.000
ZincZn %Balance
---
---
---
---
---
Heat Treatment
As Raw or Solution Heat Treated
Mechanical Properties
Tensile Strength in Mpa570 min.
Yield Strength in Mpa300 min.
Elongation in %10 min.
Reduction of Area in %-
Hardness in HV150 min.
Impact in Joule-

Cross Reference Table

Material Standard Country Grade Belong to the Industry
CuZn37Mn3Al2PbSi AFNOR NF France Rod
CW713R AFNOR NF France Rod
CuZn37Mn3Al2PbSi MSZ Hungary Rod
CW713R MSZ Hungary Rod
CuZn37Mn3Al2PbSi CSN Czech Republic Rod
CW713R CSN Czech Republic Rod
CW713R DIN Germany Rod