Material – DIN EN 1982 CuSn7Zn4Pb7-C

Standard Specification for Copper Tin Lead Alloy Castings

Group - Non Ferrous Copper Alloys

Sub Group - DIN EN 1982 CuSn7Zn4Pb7-C Copper Tin Lead Alloy Castings

Application - Intended for Valve, Pump, General Engineering, Automotive and Other Industries

Grade Belongs to the Industry - Casting

Chemical Composition
SiliconSi %0.010 max.
LeadPb %5.000 - 8.000
IronFe %0.200 max.
TinSn %6.000 - 8.000
ZincZn %2.000 - 5.000
NickelNi %2.000 max.
AluminiumAl %0.010 max.
SulphurS %0.100 max.
AntimonySb %0.300 max.
Cu + NiCu% + Ni% 81.000 - 85.000Tensile Strength in Mpa
---
---
---
---
---
Heat Treatment
As Cast
Mechanical Properties
230 min.-
Yield Strength in Mpa120 min.
Elongation in %12 min.
Reduction of Area in %-
Hardness in HBW60 min.
Impact in Joule-

Cross Reference Table

Material Standard Country Grade Belong to the Industry
CuSn7Zn4Pb7-C ONORM Australia Casting
CC493K ONORM Australia Casting
CuSn7Zn4Pb7-C BDS Bulgaria Casting
CC493K BDS Bulgaria Casting
CuSn7Zn4Pb7-C SFS Finland Casting
CuSn7Zn4Pb7-C CSN Czech Republic Casting
CuSn7Zn4Pb7-C MSZ Hungary Casting